Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 100 - 200 °C |
72.2 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 30.0 - 200 °C |
72.2 µin/in-°F @Temperature 86.0 - 392 °F |
|
3M Dyneon™ TF 4105 PTFE 25% Glass Fiber Filled
(discontinued **) Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 30.0 - 300 °C |
72.2 µin/in-°F @Temperature 86.0 - 572 °F |
|
3M Dyneon™ TFM™ 4105 Modified PTFE, 25% Glass Fiber Filled
(discontinued **) Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 30.0 - 300 °C |
72.2 µin/in-°F @Temperature 86.0 - 572 °F |
|
3M Dyneon™ TF 4406 PTFE, 60% Bronze Filled
(discontinued **) Type II PTFE. Applications include sliding surfaces, bearings.Data provided by Dyneon. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
|
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 100 - 200 °C |
72.2 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 60.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 60.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Asia Pacific) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 60.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature -40.0 - 40.0 °C |
72.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature -40.0 - 40.0 °C |
72.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature -40.0 - 40.0 °C |
72.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature -40.0 - 40.0 °C |
72.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature -40.0 - 40.0 °C |
72.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-LOY K3000Z Acetal LNP* STAT-LOY* K3000Z is a compound based on unfilled Acetal resin. Added feature of this material is: Antistat. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature -40.0 - 40.0 °C |
72.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY K3000Z Acetal LNP* STAT-LOY* K3000Z is a compound based on unfilled Acetal resin. Added feature of this material is: Antistat. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature -30.0 - 30.0 °C |
72.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature -30.0 - 30.0 °C |
72.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM D696 |
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6
(Unverified Data**) Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
|
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |