Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature <=143 °C |
7.22 µin/in-°F @Temperature <=289 °F |
Below Tg; ISO 11359 |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature >=162 °C |
7.22 µin/in-°F @Temperature >=324 °F |
Above Tg; ISO 11359 |
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, .. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature -40.0 - 150 °C |
7.22 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 23.0 - 150 °C |
7.22 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature -40.0 - 150 °C |
7.22 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 23.0 - 150 °C |
7.22 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 150 - 250 °C |
7.22 µin/in-°F @Temperature 302 - 482 °F |
2 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 23.0 - 150 °C |
7.22 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM SF2360 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 23.0 - 150 °C |
7.22 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+HIPS (Europe-Africa-Middle East) DATA ON BK1005 ONLY. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 23.0 - 150 °C |
7.22 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+PS DATA ON BK1005 ONLY. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature -40.0 - 150 °C |
7.22 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 23.0 - 150 °C |
7.22 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 180 °C |
7.22 µin/in-°F @Temperature 356 °F |
DIN 53752 |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
CTE, linear, Parallel to Flow | 13.0 µm/m-°C @Temperature 149 - 249 °C |
7.22 µin/in-°F @Temperature 300 - 480 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)