Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 10.0 µm/m-°C @Temperature <=162 °C |
5.56 µin/in-°F @Temperature <=324 °F |
Below Tg; ISO 11359 |
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, .. |
|||
CTE, linear, Parallel to Flow | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical.. |
|||
CTE, linear, Parallel to Flow | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs.. |
|||
CTE, linear, Parallel to Flow | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s.. |
|||
CTE, linear, Parallel to Flow | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
CTE, linear, Parallel to Flow | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
CTE, linear, Parallel to Flow | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
2; ISO 11359-2 |
Solvay Specialty Polymers Ryton® R-4-280BL Polyphenylene Sulfide (PPS), Glass Fiber Ryton® R-4-280BL 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis.. |
|||
CTE, linear, Parallel to Flow | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
2; ISO 11359-2 |
Solvay Specialty Polymers Ryton® R-4-280NA Polyphenylene Sulfide (PPS), Glass Fiber Ryton® R-4-280NA 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis.. |
|||
CTE, linear, Parallel to Flow | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S.. |
|||
CTE, linear, Parallel to Flow | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® XE4050BL Polyphenylene Sulfide Alloy (PPS Alloy), GlassMineral Filled Ryton® XE4050BL glass fiber and mineral filled polyphenylene sulfide alloy compound provides high ductility and impact strength along with good thermal stability.Features: Ductile; Good Thermal S.. |
|||
CTE, linear, Parallel to Flow | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta.. |