Thermal Properties | Metric | English | Comments |
---|---|---|---|
Hot Ball Pressure Test | <= 110 °C | <= 230 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Europe-Africa-Middle East) CYCOLOY LG9000 is a low gloss PC+ABS injection moulding grade. LG9000 combines good impact / heat and UV resistance with a low gloss surface appearence. It is suitable for automotive interior applic.. |
|||
Hot Ball Pressure Test | <= 110 °C | <= 230 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® C1100 PC+ABS (Europe-Africa-Middle East) CYCOLOY C1100 is a PC+ABS blend developed to satisfy the demanding application requirements, where optimum combination is needed of superior processing efficiency, excellent ductility also at sub ze.. |