Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 313 °C | 595 °F | |
Indium Corp. Indalloy 11 Lead Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 313 °C | 595 °F | |
Indium Corp. Indalloy® 239 Pb-Ag-Sn-In Solder Alloy High temp solder.Information provided by the manufacturer, Indium Corporation. |