Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 216 °C | 421 °F | |
Indium Corp. Indalloy 119 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 216 °C | 421 °F | |
Johnson Matthey JM5050 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |