Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1855 °C | 3371 °F | |
Goodfellow Platinum 90/Rhodium 10 Thermocouple Alloy The positive element of the type S thermocouple. Type S thermocouples are characterized by a high degree of chemical inertness and stability at high temperatures. Often used as a standard for calibr.. |