Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1355 °C | 2471 °F | |
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
Liquidus | 1355 °C | 2471 °F | |
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
Liquidus | 1355 °C | 2471 °F | |
HP Alloys Alloy X, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, and Haynes International. |
|||
Liquidus | 1355 °C | 2471 °F | |
Special Metals INCONEL® HX Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Liquidus | 1355 °C | 2471 °F | |
Special Metals NIMONIC® Alloy 263 A precipitation-hardenable nickel-chromium-cobalt alloy with an addition of molybdenum for solid-solution strengthening. It has high strength and corrosion resistance along with good formability an.. |
|||
Liquidus | 1355 °C | 2471 °F | |
Special Metals NIMONIC® Alloy PE16 A precipitation-hardenable nickel-iron-chromium alloy with an addition of molybdenum for solid-solution strengthening. It has good strength and oxidation resistance at temperatures to about 1380°.. |
|||
Liquidus | 1355 °C | 2471 °F | |
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening.. |
|||
Liquidus | 1355 °C | 2471 °F | |
Special Metals INCONEL® Alloy HX A nickel-chromium-iron-molybdenum alloy with outstanding strength and oxidation resistance at temperatures to 2200°F (1200°C). Matrix stiffening provided by the molybdenum content results in high.. |
|||
Liquidus | 1355 °C | 2471 °F | |
HP Alloys Alloy X, 15% Cold Worked 15% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, and Haynes International. |
|||
Liquidus | 1355 °C | 2471 °F | |
HP Alloys Alloy X, 5% Cold Worked 5% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, and Haynes International. |