Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 971 °C | 1780 °F | Flow Point |
Lucas-Milhaupt BRAZE 852 Silver Based Cadmium Free Filler Metal Characteristics: Braze 852 is a high temperature, free flowing silver brazing filler metal usable both for torch and atmosphere furnace brazing. Due to the high flow point of this alloy, torch brazi.. |
|||
Liquidus | 971 °C | 1780 °F | |
Universal Wire Works BAg-23 (AMS 4766) Silver Brazing Filler Metal Information provided by Universal Wire Works for their line of welding wire and filler metal. |
|||
Liquidus | 970 °C | 1780 °F | |
Williams Advanced Alloys Wambraze™ WB970 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |