Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1675 °C | 3047 °F | |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 10% Equiaxed Alpha + Annealed This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 10% Equiaxed Alpha + Annealed (705°C/1hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4-6. .. |
|||
Liquidus | 1675 °C | 3047 °F | |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 10% Equiaxed Alpha + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 10% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®.. |
|||
Liquidus | 1675 °C | 3047 °F | |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 20% Elongated Alpha + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 20% Elongated Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL.. |
|||
Liquidus | 1675 °C | 3047 °F | |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Elongated Alpha + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Elongated Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL.. |
|||
Liquidus | 1675 °C | 3047 °F | |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + Annealed This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + Annealed (705°C/1hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4-6. .. |
|||
Liquidus | 1675 °C | 3047 °F | |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®.. |
|||
Liquidus | 1675 °C | 3047 °F | |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STOA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STOA (885°C/1hr/AC + 705°C/1hr/AC) condition. Other data below are typical of TIMETAL.. |
|||
Liquidus | 1675 °C | 3047 °F | |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Typical This entry has typical property data. Other database entries for TIMETAL® 6-2-4-6 have tensile and fatigue data for specific sample conditions.High-Strength, Intermediate Temperature AlloyFeatures.. |
|||
Liquidus | 1675 °C | 3047 °F | |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Beta Forged + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the Beta Forged + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4.. |