Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 150 °C | 302 °F | |
Indium Corp. Indalloy 88 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 150 °C | 302 °F | Flow Point |
Aremco Crystalbond™ 590 Washaway Mounting Adhesive & Accessory High strength, resilient adhesive system, ideal for dicing miniature and tall parts. Soluble in methanol or 590-S stripper, a water-dispersible, environmentally-safe powder concentrate. |
|||
Liquidus | 150 °C | 302 °F | |
Indium Corp. Indalloy 203 Indium Solder Alloy Information Provided by Indium Corporation |