Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1370 °C | 2500 °F | |
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Haynes HR-160® alloy plate, aged 4000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Haynes HR-160® alloy, annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Haynes HR-160® alloy, plate, aged 1000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Haynes HR-160® alloy, plate, aged 4000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Haynes HR-160® alloy, plate, aged 8000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Liquidus | 1370 °C | 2500 °F | |
HP Alloys Alloy C-276, 10% Cold Worked 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Liquidus | 1370 °C | 2500 °F | |
HP Alloys Alloy C-276, 20% Cold Worked 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Liquidus | 1370 °C | 2500 °F | |
HP Alloys Alloy C-276, 40% Cold Worked 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Liquidus | 1370 °C | 2500 °F | |
HP Alloys Alloy C-276, 50% Cold Worked 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Special Metals INCONEL® Alloy C-276 A nickel-molybdenum-chromium alloy with an addition of tungsten having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially .. |
|||
Liquidus | 1370 °C | 2500 °F | |
Special Metals INCONEL® C276 Nickel Superalloy Bar Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed bar. Other property values are typical of INCO® C276.Data provided by the manufacturer, Special .. |
|||
Liquidus | 1370 °C | 2500 °F | |
Special Metals INCONEL® C276 Nickel Superalloy Plate Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed plate. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Special Metals INCONEL® C276 Nickel Superalloy Sheet Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed sheet. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 0% Cold Work (Annealed) Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed tubing. Other property values are typical of INCO® C276.Data provided by the manufacturer, Speci.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 24% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 24% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 27% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 27% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 30% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 30% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Liquidus | 1370 °C | 2500 °F | |
Special Metals NIMONIC® Alloy 90 A precipitation-hardenable nickel-chromium-cobalt alloy having high stress-rupture strength and creep resistance at temperatures to about 1700°F (920°C). The alloy also has good resistance to.. |
|||
Liquidus | 1370 °C | 2490 °F | |
Weartech International WT-21 Cobalt Hardfacing & Wear Resistant Alloy Applications: hot trimming & forging dies, high pressure high temperature valves, hot shears, valve seats, pump impellers, ringsInformation provided by Weartech International |
|||
Liquidus | 1370 °C | 2500 °F | |
Carlson GOC 276 Nickel-Molybdenum-Chromium General DescriptionCarlson Alloy GOC 276 is a nickel-molybdenum-chromium alloy exhibiting outstanding corrosion resistance over a wide range of service environments. This alloy is generally use in .. |
|||
Liquidus | 1370 °C | 2500 °F | |
HP Alloys Alloy C-276, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |