Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1366 °C | 2491 °F | |
Kennametal Stellite Stellite® 21 Excellent high temperature strength, high toughness. Solution treat at 1191-1204°C, rapid air cool, age between 538-871°C to increase hardness and strength at the expense of impact and ducti.. |
|||
Liquidus | 1366 °C | 2491 °F | |
Special Metals INCOLOY® Alloy 925 A precipitation-hardenable nickel-iron-chromium alloy with additions of molybdenum and copper. It combines the high strength of a precipitation-hardenable alloy with the excellent corrosion resista.. |