Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 268 °C | 514 °F | |
Williams Advanced Alloys WS286 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 268 °C | 514 °F | |
Williams Advanced Alloys WS290 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 268 °C | 514 °F | |
Johnson Matthey JM1090 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |