Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 1840 °C | 3340 °F | |
Wieland 1744 Wilaform Platinum Hard platinum alloy for strongly stressed decorationApplications: chains, laminar decoration, pipes, tubingDental |
|||
Solidus | 1840 °C | 3340 °F | |
Goodfellow Platinum 87/Rhodium 13Thermocouple Alloy The positive element of the type R thermocouple. Type R thermocouples are used when chemical inertness and stability at high temperatures, up to 1750C, are required.Information provided by Goodfello.. |