Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 1110 °C
2030 °F
Wieland 1907 Wilaform Gold
Palladium white gold alloy with beautiful grey-white color.Applications: casting, chains, laminar decoration, pipes, tubingDental
Solidus 1110 °C
2030 °F
Wieland 1916 Wilaform Gold
Hard palladium white gold alloy with beautiful grey color.Applications: casting, chains, laminar decoration, pipes, tubingDental