Polymer Property : Solidus = 1220 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 660 °C
1220 °F
Indium Corp. Indalloy 192 Pure Aluminum
Information Provided by Indium Corporation
Solidus 660 °C
1220 °F
Johnson Matthey Argo-braze 502 Silver Brazing Alloy for Tungsten Carbide Brazing
These products are specifically designed for brazing of tungsten carbide tips to steel tools and wear parts. Optimum Joint Gap 0.1 - 0.25 mm.AMS 4788AWS A5.8-92 BAg-24Equivalent to Engelhard Silvalo..
Solidus 660 °C
1220 °F
Melting Point
Lucas-Milhaupt BRAZE 505 Carbide Brazing Alloy
Applications: Braze 505 readily wets nickel and iron base alloys. It is recommended for joining 300 Series stainless steel and will retard interface corrosion in most exposures for which the base m..
Solidus 660 °C
1220 °F
Lucas-Milhaupt Silvaloy® A50N Flux Coated Rod Brazing Alloy
Silvacote A50N Flux Cored is a cadmium free silver brazing alloy that has found numerous applications for joining 300 series stainless steel in food, medical, and dental fields. Addition of nickel t..
Solidus 660 °C
1220 °F
Lucas-Milhaupt Silvacore® A50N Flux Cored Brazing Alloy
Silvacote A50N Flux Coated Rod is a cadmium free silver brazing alloy that has found numerous applications for joining 300 series stainless steel in food, medical, and dental fields. Addition of nic..
Solidus 660 °C
1220 °F
Lucas-Milhaupt Silvacote® A50N Brazing Alloy
Silvacote A50N is a cadmium free silver brazing alloy that has found numerous applications for joining 300 series stainless steel in food, medical, and dental fields. Addition of nickel to the silve..
Solidus 660 °C
1220 °F
Johnson Matthey Argo-braze 40N Silver Brazing Alloy for Tungsten Carbide Brazing
An economical alloy for brazing tungsten carbides and stainless steels. Optimum Joint Gap 0.1 - 0.25 mm.AWS A5.8-92 BAg-4Federal Specification QQ-B-564 BAg-4Information provided by Johnson Matthey.
Solidus 660 °C
1220 °F
Johnson Matthey Matti-sil 38Sn Cadmium Free Brazing Alloy
An economic alternative to Matti-sil 40Sn with similar properties.Optimum Joint Gap 0.075 - 0.2 mm.AMS 4761AWS A5.8-92 BAg-34Equivalent to Engelhard Silvaloy A-38TEquivalent to Handy & Harman Braze ..