Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 567.2 - 573.2 °C | 1053 - 1064 °F | |
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |