Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 980 °C | 1800 °F | |
Osprey Metals HTN 1A Brazing Powder Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme.. |
|||
Solidus | 980 °C | 1800 °F | |
Osprey Metals HTN 3 Brazing Powder Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme.. |
|||
Solidus | 980 °C | 1800 °F | |
Osprey Metals HTN 4 Brazing Powder Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme.. |
|||
Solidus | 980 °C | 1800 °F | |
Osprey Metals HTN 8 Brazing Powder Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme.. |
|||
Solidus | 980 °C | 1800 °F | |
Osprey Metals Ni 401 Brazing Powder Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme.. |
|||
Solidus | 980 °C | 1800 °F | |
Kennametal Stellite Nucalloy® 453 High-Silicon Nickel-Base Hardfacing Alloy Applications include chemical control valves, nuclear globe valves, nuclear gate valves, nuclear sliding parts, and pressure bars for plywood cutters.Nucalloy® alloys are unique, patented, high-s.. |
|||
Solidus | 980 °C | 1800 °F | |
Wieland 1909 Wilaform Gold Hard palladium white gold alloy with beautiful white color.Applications: casting, chains, laminar decoration, pipes, tubingDental |
|||
Solidus | 980 °C | 1800 °F | |
CMW® 28 Copper Alloy CMW® 28 material is a copper base alloy having very high electrical and thermal conductivity and medium strength and toughness. It is a heat treatable alloy and develops its strength and hardness t.. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® 1060 Silver Tungsten Carbide Contact Material Electrical contactor material for medium current ac applicationsInformation provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® 20S Infiltrated Tungsten Silver Contact Material ASTM B531, Class A, infiltrated For electrical contacts resistant to arcing and welding in circuit breakers, etc.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® 2150 Silver Tungsten contact material ASTM B631, Class C, press-sinter-repress For electrical ContactsInformation provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® 2188 Infiltrated Tungsten Silver Contact Material High wear resistance and reliability.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® 3042 Silver Tungsten Carbide contact material ASTM B663 For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® 30S Silver Tungsten contact material ASTM B631 For electrical contacts, circuit breakers. Resistant to arcing and welding.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® 3150 Silver Tungsten Carbide contact material ASTM B663 Table 2, Class B For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® 35S Silver Tungsten contact material ASTM B631, Class B, infiltrated For arcing and current carrying electrical contacts; household and power circuit breakers.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® 40S Infiltrated Tungsten Silver contact material ASTM B631 For arcing and current carrying electrical contacts.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® 45S Infiltrated Tungsten Silver contact material ASTM B631 For arcing and current carrying electrical contacts.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® 50S Infiltrated Tungsten Silver contact material ASTM B631, Class C, infiltrated For arcing and current carrying electrical contacts.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® 7065 Infiltrated Molybdenum Silver contact material ASTM B662 Table 1, Class A1 For arcing electrical contactsInformation provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® 7165 Molybdenum Silver contact material For arcing electrical contactsInformation provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® G13 Tungsten Carbide Silver contact material ASTM 663, Class B, infiltrated For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® G14 Tungsten Carbide Silver contact material ASTM 663, Class A, infiltrated For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® G17 Molybdenum Silver contact material ASTM 662, Class A, infiltrated For arcing electrical contacts especially where low mass is required.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® G18 Molybdenum Silver contact material ASTM 662, Class B, infiltrated For arcing electrical contacts especially where low mass is required.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® TC10 Tungsten Carbide Copper material For wiping and arcing electrical contacts and projection welding tips.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® TC20 Tungsten Carbide Copper material For electroforging and electrical upsetting dies.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® TC5 Tungsten Carbide Copper material For wiping and arcing electrical contacts and light duty welding tips.Information provided by CMW Inc. |
|||
Solidus | 980 °C | 1800 °F | |
CMW® ELKONITE® TC53 Heat Treatable Tungsten Carbide Copper material For electroforging and electrical upsetting dies.Information provided by CMW Inc. |