Solidus 690.6 °C
1275 °F
Melting Point
Lucas-Milhaupt BRAZE 630 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 630 is very sluggish because of its wide melting range, and will bridge wide or irregular joint clearances. To avoid liquation (separation and flow of the low-melting compon..
Solidus 690.6 °C
1275 °F
Melting Point
Lucas-Milhaupt BRAZE 700 (Medium) Silver Based Cadmium Free Filler Metal
Characteristics: This alloy is a intermediate silver brazing filler metals with a slight tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through their mel..
Solidus 690.6 °C
1275 °F
Universal Wire Works BAg-18 (AMS 4774) Silver Brazing Filler Metal
Information provided by Universal Wire Works for their line of welding wire and filler metal.