Polymer Property : Solidus = 308 °C
Polymer Property :
Solidus =
308 °C
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Solidus
308
°C
586
°F
Indium Corp. Indalloy® 171 Pb-Sn Solder Alloy
Wide application in soldering.Information provided by the manufacturer, Indium Corporation.