Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 230 °C | 446 °F | |
Johnson Matthey JM 97C Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Solidus | 230 °C | 446 °F | |
Johnson Matthey JM 99C Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |