Solidus 1351 °C
2464 °F
Special Metals INCONEL® alloy 22 Austenitic Alloy
INCONEL® alloy 22 (UNS N06022; W.Nr. 2.4602; NiCr21Mo14W) is a fully austenitic advanced corrosion-resistant alloy that offers resistance to both aqueous corrosion and attack at elevated temperat..