Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Solidus = 1075 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 1075 °C
1967 °F
Kennametal Stellite Nucalloy® 488V High-Silicon Nickel-Base Hardfacing Alloy
Applications include diesel engine valves, and injection mold screws.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinati..
Solidus 1075 °C
1967 °F
CMW® 328 Copper Alloy
CMW® 328 material is a high strength, high conductivity copper base alloy. CMW® 328 is heat treatable. Optimum mechanical and physical properties of CMW® 328 material are developed by heat treatm..