Polymer Property : Thermal Conductivity = 9.16 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.22 - 1.32 W/m-K

@Temperature 1000 °C
8.47 - 9.16 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 120 S Dense Refractory Castable
Description: A very strong castable with a high abrasion resistance of which both aggregate and cement attribute to hydraulic binding.Remarks: These values apply to cast products. Also available in ..