Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.270 - 0.370 W/m-K @Temperature 200 °C |
1.87 - 2.57 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Gouda Vuurvast GI 28 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.270 - 0.370 W/m-K @Temperature 1000 °C |
1.87 - 2.57 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Informati.. |
|||
Thermal Conductivity | 0.270 - 0.370 W/m-K @Temperature 1260 °C |
1.87 - 2.57 BTU-in/hr-ft²-°F @Temperature 2300 °F |
|
Gouda Vuurvast GOLITE 135 L Refractory Insulating Castable Description: Golite 135 L can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning va.. |