Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.220 - 0.300 W/m-K @Temperature 100 °C |
1.53 - 2.08 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 1.2.4. Mix Refractory Insulating Castable Description: This lightweight castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Remarks: Th.. |
|||
Thermal Conductivity | 0.200 - 0.300 W/m-K @Temperature 100 °C |
1.39 - 2.08 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Informati.. |
|||
Thermal Conductivity | 0.220 - 0.300 W/m-K @Temperature 950 °C |
1.53 - 2.08 BTU-in/hr-ft²-°F @Temperature 1740 °F |
|
Gouda Vuurvast GOLITE 95 Refractory Insulating Castable Description: Golite 95 is widely applied as an insulating backlining behind a dense castable, especially in the petrochemical industry.Remarks: These values apply to cast products. Also available in.. |