Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.00 - 2.20 W/m-K @Temperature 100 °C |
13.9 - 15.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURASBOND 85 Moldable Refractory Material Description: Curasbond 85 is a pouring repairmass, characterized by excellent resistance to aluminum and rapid hardening. The product is supplied in two components: a dry powder and a liquid. It can.. |
|||
Thermal Conductivity | 1.80 - 2.20 W/m-K @Temperature 100 °C |
12.5 - 15.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 180 Refractory Insulating Castable Description: Hollow alumina spheres are used as an aggregate for this castable. With very low percentages of Fe2O3 and SiO2, it is well resistant against reducing and corrosive kiln atmospheres.Rema.. |
|||
Thermal Conductivity | 2.00 - 2.20 W/m-K @Temperature 1600 °C |
13.9 - 15.3 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Gouda Vuurvast FLUCON 180 Dense Self Flowing Refractory Castable Description: Flucon 180 is a self flowing castable based on white fused Alumina. This castable is applied at severe thermal conditions and or severe slag attack.Remarks: These values apply to cast p.. |