Thermal Properties Metric English Comments
Thermal Conductivity 0.160 - 0.240 W/m-K

@Temperature 600 °C
1.11 - 1.67 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 1.0.6. Mix Refractory Insulating Castable
Description: This castable is composed of a high quality alumina cement and vermiculite and is applied as a backlining. Special additives are responsible for the low shrinkage. This castable can be ..