Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 13.89 W/m-K @Temperature 300 °C |
96.37 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Stellar Canada CERAMITE® CSA Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |