Polymer Property : Thermal Conductivity = 90.2 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 13.0 W/m-K

@Temperature 100 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 212 °F
Special Metals INCOLOY® alloy 864
INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma..
Thermal Conductivity 13.0 W/m-K

@Temperature 20.0 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate
This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers
Thermal Conductivity 13.0 W/m-K

@Temperature 20.0 - 100 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum AL 4565™ Corrosion Resistant Stainless Steel
Characteristics:Very high resistance to pitting and crevice corrosion Excellent general corrosion resistance in a variety of media Higher mechanical propertied then conventional stainless steels Go..