Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.41 W/m-K @Temperature 650 °C |
9.79 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 53 E Dense Refractory Brick Description: Because of its very high erosion resistance this brick is applied in e.g. recirculation cyclones for CFB coal fired boilers.Remarks: This data represents average values, obtained from s.. |
|||
Thermal Conductivity | 1.41 - 1.42 W/m-K @Temperature 1600 °C |
9.79 - 9.85 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Gouda Vuurvast CURON 180 T SP GM Dense Refractory Castable Description: Curon 180 T SP GM is a gunning castable based on tabular alumina for application at very high temperatures.Remarks: These values apply to cast products.Information provided by Gouda Vuu.. |