Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.31 - 1.51 W/m-K @Temperature 100 °C |
9.09 - 10.5 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 90 D Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This high refractory ramming material contains several well defined corund.. |
|||
Thermal Conductivity | 1.31 - 1.41 W/m-K @Temperature 600 °C |
9.09 - 9.79 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 170 Dense Refractory Castable Description: A general purpose castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks: These v.. |
|||
Thermal Conductivity | 1.31 - 1.41 W/m-K @Temperature 600 °C |
9.09 - 9.79 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 170 GM Dense Refractory Castable Description: A general purpose gunning castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks:.. |