Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 120 W/m-K @Temperature 25.0 °C |
833 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Osprey Metals CE7 Al-Si Controlled Expansion Alloy Si-30%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
Thermal Conductivity | 120 W/m-K @Temperature 100 °C |
833 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Thermal Conductivity | 120 W/m-K @Temperature 20.0 - 100 °C |
833 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
DIN EN 821-2 / ASTM-C408 |
CeramTec Rocar® SiF Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Thermal Conductivity | 120 W/m-K @Temperature 20.0 °C |
833 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
hardened to 30 HRC |
Bohler-Uddeholm BeCu Alloy 172 Mold Material Beryllium copper alloyA high strength beryllium copper mold alloy with high thermal conductivity.BeCu Alloy 172 is characterized by: High thermal conductivity Good corrosion resistance Good polisha.. |