Polymer Property : Thermal Conductivity = 8.47 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.22 - 1.42 W/m-K

@Temperature 1100 °C
8.47 - 9.85 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast CURAS 60 S Moldable Refractory Material
Description: Because this material contains a high percentage of sillimanite, it has a very good thermal shock resistance together with a very good slag resistance. Therefore this material finds its..
Thermal Conductivity 1.22 - 1.32 W/m-K

@Temperature 1000 °C
8.47 - 9.16 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 120 S Dense Refractory Castable
Description: A very strong castable with a high abrasion resistance of which both aggregate and cement attribute to hydraulic binding.Remarks: These values apply to cast products. Also available in ..
Thermal Conductivity 1.22 W/m-K

@Temperature 400 °C,
Time 10800 sec
8.47 BTU-in/hr-ft²-°F

@Temperature 752 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST 80 High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Thermal Conductivity 1.22 W/m-K

@Temperature 600 °C,
Time 10800 sec
8.47 BTU-in/hr-ft²-°F

@Temperature 1110 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST LC45 Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Thermal Conductivity 1.22 - 1.42 W/m-K

@Temperature 600 °C
8.47 - 9.85 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 180 Refractory Insulating Castable
Description: Hollow alumina spheres are used as an aggregate for this castable. With very low percentages of Fe2O3 and SiO2, it is well resistant against reducing and corrosive kiln atmospheres.Rema..