Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 110 W/m-K @Temperature 20.0 °C |
763 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
hardened to 40 HRC |
Bohler-Uddeholm BeCu Alloy 172 Mold Material Beryllium copper alloyA high strength beryllium copper mold alloy with high thermal conductivity.BeCu Alloy 172 is characterized by: High thermal conductivity Good corrosion resistance Good polisha.. |