Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, 10% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, 50% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, 60% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, GMAW short arc HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW weld, C-22 base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW, as welded, notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, SMAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GMAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GTAW weldment, sheet - plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 500 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber Description: Manufactured near-oxygen-free using electron-beam curing. The fiber is homogeneously composed of ultrafine beta-SiC crystallites and carbon. The fiber has excellent strength and modulus.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, SMAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, GMAW, as welded, unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW weld, 904L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW, as welded, unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GTAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, SMAW weldment, 19.1 mm thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 23.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 10 hours at 649°C (1200°F) Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 23.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, 6.4-19.1 mm thick plate, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, GMAW, aged 4000 hours at 450°C (800°F), notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, GMAW, aged 4000 hours at 450°C (800°F), unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Thermal Conductivity | 10.1 W/m-K @Temperature 48.0 °C |
70.1 BTU-in/hr-ft²-°F @Temperature 118 °F |
|
Haynes Hastelloy® C-22® alloy, SMAW weld, 904L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |