Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.06 W/m-K @Temperature 260 °C |
7.36 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Pyrotek Pyrocast AR-S Castable Refractory Pyrocast AR-S is a low cement, fused silica, castable refractory which exhibits excellent resistance to thermal shock. It is inert to liquid aluminum and its alloys. It is a high strength material.. |