Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 10.0 W/m-K @Temperature 25.0 °C |
69.4 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 10.0 W/m-K @Temperature 25.0 °C |
69.4 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 10.0 W/m-K @Temperature 25.0 °C |
69.4 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 10.0 W/m-K @Temperature 25.0 °C |
69.4 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 10.0 W/m-K @Temperature 25.0 °C |
69.4 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Thermal Conductivity | 10.0 W/m-K @Temperature 25.0 °C |
69.4 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Thermal Conductivity | 10.0 W/m-K @Temperature 25.0 °C |
69.4 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |