Thermal Properties Metric English Comments
Thermal Conductivity 0.780 W/m-K

@Temperature 550 °C
5.41 BTU-in/hr-ft²-°F

@Temperature 1020 °F
Pyrotek Pyrocast AR PLUS Castable Refractory
Pyrocast AR Plus is a fused silica refractory castable inert to molten aluminum and its alloys. Parts cast from Pyrocast AR Plus are heat-treated to ensure that free and combined water are removed...
Thermal Conductivity 0.780 - 0.880 W/m-K

@Temperature 1300 °C
5.41 - 6.11 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURON 160 HF Dense Refractory Castable
Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the ..
Thermal Conductivity 0.780 - 0.880 W/m-K

@Temperature 100 °C
5.41 - 6.11 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 13 S Dense Refractory Castable
Description: Curon 13 S is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/hol..
Thermal Conductivity 0.780 - 0.880 W/m-K

@Temperature 100 °C
5.41 - 6.11 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 13 SC Dense Refractory Castable
Description: Curon 13 SC is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/ho..
Thermal Conductivity 0.780 - 0.880 W/m-K

@Temperature 100 °C
5.41 - 6.11 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 14 S Dense Refractory Castable
Description: Curon 14 S is a dense, strong and abrasion resistant castable. Because of the very low percentage of Fe2O3 and SiO2 it is used for highly abrasive conditions in reducing atmospheres.Rem..
Thermal Conductivity 0.780 W/m-K

@Temperature 815 °C
5.41 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Pyrotek Pyrocast TG Castable Refractory
Pyrocast TG is a technical-grade silica based refractory developed for the non-ferrous industry including nickel, copper, zinc, and their alloys.ApplicationsCoreless induction furnace lining Channel..
Thermal Conductivity 0.780 - 0.880 W/m-K

@Temperature 1500 °C
5.41 - 6.11 BTU-in/hr-ft²-°F

@Temperature 2730 °F
Gouda Vuurvast GOLITE 180 Refractory Insulating Castable
Description: Hollow alumina spheres are used as an aggregate for this castable. With very low percentages of Fe2O3 and SiO2, it is well resistant against reducing and corrosive kiln atmospheres.Rema..