Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 6.82 W/m-K @Temperature 25.0 °C |
47.3 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Mateck Quartz Crystalline (SiO2) Optical crystals |