Thermal Conductivity 0.610 - 0.710 W/m-K

@Temperature 600 °C
4.23 - 4.93 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 150 AC Dense Refractory Castable
Description: Curon 150 AC is a coarse castable for use up to 1500°C with a high strength.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.610 - 0.710 W/m-K

@Temperature 100 °C
4.23 - 4.93 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 160 HF Dense Refractory Castable
Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the ..
Thermal Conductivity 0.610 - 0.710 W/m-K

@Temperature 100 °C
4.23 - 4.93 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 160 HS Dense Refractory Castable
Description: Because of the selection of raw materials, this castable has a high volume stability and a high strength up to high temperatures. In addition, Curon 160 HS has an excellent thermal shoc..
Thermal Conductivity 0.610 - 0.710 W/m-K

@Temperature 100 °C
4.23 - 4.93 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable
Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva..
Thermal Conductivity 0.610 W/m-K

@Temperature 600 °C
4.23 BTU-in/hr-ft²-°F

@Temperature 1110 °F
parallel to thickness; ASTM C1113
Zircar Refractory Composites RSLE-501 CYLINDERS Refractory Sheet
ZIRCAR Refractory Sheet Type RSLE-501 is a low expansion high strength reinforced silica matrix composites in a cylindrical form. This material was designed for use as a high strength, durable insul..
Thermal Conductivity 0.610 W/m-K

@Temperature 600 °C
4.23 BTU-in/hr-ft²-°F

@Temperature 1110 °F
parallel to thickness; ASTM C1113
Zircar Refractory Composites RSLE-56 MOLDABLE Refractory Sheet
ZIRCAR Refractory Sheet Type RSLE-56 Moldable is a high silica fiber reinforced ceramic composite material that is easily cut and formed into flat sheets in addition to a wide variety of simple and ..
Thermal Conductivity 0.610 W/m-K

@Temperature 600 °C
4.23 BTU-in/hr-ft²-°F

@Temperature 1110 °F
parallel to thickness; ASTM C1113
Zircar Refractory Composites RSLE-57 Refractory Sheet
ZIRCAR Refractory Sheet Type RSLE-57 is a low expansion high strength reinforced silica matrix composite . This material was designed for use as a high strength insulator in induction hot press appl..
Thermal Conductivity 0.610 W/m-K

@Temperature 295 °C
4.23 BTU-in/hr-ft²-°F

@Temperature 563 °F
Pyrotek Pyrocast TG Castable Refractory
Pyrocast TG is a technical-grade silica based refractory developed for the non-ferrous industry including nickel, copper, zinc, and their alloys.ApplicationsCoreless induction furnace lining Channel..
Thermal Conductivity 0.610 - 0.710 W/m-K

@Temperature 100 °C
4.23 - 4.93 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 165 Dense Refractory Castable
Description: Curon 165 is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Also availa..
Copyright © lookpolymers.com All Rights Reserved