Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.460 W/m-K @Temperature 607 °C |
3.19 BTU-in/hr-ft²-°F @Temperature 1120 °F |
hot face 744°C, cold face 470°C, mean - 607°C |
Pyrotek Insural® 140 Insulating Refractory Shapes for Aluminum Insural® 140 Precast Shapes are designed for the containment of molten aluminum in hot top modules (cross feeder) and trough/launder applications.AdvantagesNear zero expansion avoids gaps at the jo.. |
|||
Thermal Conductivity | 0.460 - 0.560 W/m-K @Temperature 1370 °C |
3.19 - 3.89 BTU-in/hr-ft²-°F @Temperature 2500 °F |
|
Gouda Vuurvast GOLITE 140 Refractory Insulating Castable Description: This castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere.Remarks:.. |
|||
Thermal Conductivity | 0.460 - 0.560 W/m-K @Temperature 1370 °C |
3.19 - 3.89 BTU-in/hr-ft²-°F @Temperature 2500 °F |
|
Gouda Vuurvast GOLITE 140 GM Refractory Insulating Castable Description: This gunning castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere... |