Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 33.0 W/m-K @Temperature 500 °C |
229 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st.. |
|||
Thermal Conductivity | 33.0 W/m-K @Temperature 399 °C |
229 BTU-in/hr-ft²-°F @Temperature 750 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM QRO® 90 SUPREME Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelQRO® 90 SUPREME is a premium hot work die steel with high hot yield strength and very good temper resistance. Especially suited for die casting of aluminum.. |
|||
Thermal Conductivity | 33.0 W/m-K @Temperature 599 °C |
229 BTU-in/hr-ft²-°F @Temperature 1110 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM QRO® 90 SUPREME Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelQRO® 90 SUPREME is a premium hot work die steel with high hot yield strength and very good temper resistance. Especially suited for die casting of aluminum.. |
|||
Thermal Conductivity | 33.0 W/m-K @Temperature 200 °C |
229 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Assab Steels DF-3 Cold Work Steel DF-3 general purpose oil-hardening tool steel is a versatile manganese-chromium-tungsten steel suitable for a wide variety of cold-work applications. Its main characteristics include:Good machinabil.. |
|||
Thermal Conductivity | 33.0 W/m-K @Temperature 400 °C |
229 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Assab Steels HOTVAR Hot Work Steel HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue.. |
|||
Thermal Conductivity | 33.0 W/m-K @Temperature 600 °C |
229 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Assab Steels HOTVAR Hot Work Steel HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue.. |
|||
Thermal Conductivity | 33.0 W/m-K @Temperature 500 °C |
229 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum AL 304DA Stainless/Carbon Steel Three-Ply Composite Composition above represents only the Type 304 cladding. Its iron content calculated as balance.Allegheny Ludlum AL 304DA is tri-ply composite consisting of a dual stabilized, low carbon steel cent.. |
|||
Thermal Conductivity | 33.0 W/m-K @Temperature 191 °C |
229 BTU-in/hr-ft²-°F @Temperature 375 °F |
hardened to 62 HRC |
Bohler-Uddeholm O1 Cold Work Tool Steel Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha.. |