Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 31.1 W/m-K @Temperature 427 °C |
216 BTU-in/hr-ft²-°F @Temperature 800 °F |
|
Schmolz + Bickenbach P-20 High Hard Plastic Mold Steel Description: P-20 High Hard is an improved pre-hardened mold steel that has been specially designed for large plastic molds; Material is forged on a 5000 ton press assuring maximum deformation durin.. |
|||
Thermal Conductivity | 31.1 W/m-K @Temperature 427 °C |
216 BTU-in/hr-ft²-°F @Temperature 800 °F |
|
Schmolz + Bickenbach P-20 Modified Plastic Mold Steel Description: P-20 Modified is an improved pre-hardened mold steel that has been specially designed for large plastic molds; The material is forged on a 5000 ton press assuring maximum deformation du.. |
|||
Thermal Conductivity | 31.1 W/m-K @Temperature 399 °C |
216 BTU-in/hr-ft²-°F @Temperature 750 °F |
|
EDRO #3 Prehardened Mold Quality P20 Alloy Steel EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with.. |
|||
Thermal Conductivity | 31.1 W/m-K @Temperature 600 °C |
216 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER M268 VMR® Plastic Mold Steel Description: HBÖHLER M268 VMR is a hardened and tempered plastic mould steel with excellent cleanliness for best polishability. The hardness is constant over the entire cross-section of the steel b.. |
|||
Thermal Conductivity | 31.1 W/m-K @Temperature 300 °C |
216 BTU-in/hr-ft²-°F @Temperature 572 °F |
Hardened and tempered |
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava.. |
|||
Thermal Conductivity | 31.1 W/m-K @Temperature 400 °C |
216 BTU-in/hr-ft²-°F @Temperature 752 °F |
Hardened and tempered |
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava.. |
|||
Thermal Conductivity | 31.1 W/m-K @Temperature 399 °C |
216 BTU-in/hr-ft²-°F @Temperature 750 °F |
|
Schmolz + Bickenbach Holder Block Plastic Mold Steel Description: Holder Block is a modified AISI-4130 material with higher chromium and molybdenum content specifically designed holder steel for molds and dies and The material is forged on a 5000 ton.. |