Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 30.5 W/m-K @Temperature 600 °C |
212 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E.. |
|||
Thermal Conductivity | 30.6 W/m-K @Temperature 200 °C |
212 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 468°C Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c.. |
|||
Thermal Conductivity | 30.6 W/m-K @Temperature 200 °C |
212 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 482°C Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c.. |
|||
Thermal Conductivity | 30.5 W/m-K @Temperature 250 °C |
212 BTU-in/hr-ft²-°F @Temperature 482 °F |
Quenched and Tempered |
Schmolz + Bickenbach Cryodur® 2767 Cold Work Die Steel Description: High hardenability and toughness, highly suitable for polishing, texturing and EDM machining. We recommend the use of Cryodur® 2767 (ERS) for extreme demandsApplications: Cutlery dies,.. |