Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 29.1 W/m-K @Temperature 21.1 °C |
202 BTU-in/hr-ft²-°F @Temperature 70.0 °F |
|
Schmolz + Bickenbach P-20 High Hard Plastic Mold Steel Description: P-20 High Hard is an improved pre-hardened mold steel that has been specially designed for large plastic molds; Material is forged on a 5000 ton press assuring maximum deformation durin.. |
|||
Thermal Conductivity | 29.1 W/m-K @Temperature 21.1 °C |
202 BTU-in/hr-ft²-°F @Temperature 70.0 °F |
|
Schmolz + Bickenbach P-20 Modified Plastic Mold Steel Description: P-20 Modified is an improved pre-hardened mold steel that has been specially designed for large plastic molds; The material is forged on a 5000 ton press assuring maximum deformation du.. |
|||
Thermal Conductivity | 29.1 W/m-K @Temperature 20.0 °C |
202 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
EDRO #3 Prehardened Mold Quality P20 Alloy Steel EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with.. |
|||
Thermal Conductivity | 29.1 W/m-K @Temperature 20.0 °C |
202 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
EDRO #7 Shock Resistant S7 Tool Steel EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s.. |
|||
Thermal Conductivity | 29.1 W/m-K @Temperature 20.0 °C |
202 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Assab Steels 618 Plastic Mold Material ASSAB 618 is a vacuum-degassed Cr-Ni-Mo-alloy steel which is supplied in the hardened and tempered condition. ASSAB 618 is manufactured to consistently high quality standards with a controlled sulfu.. |
|||
Thermal Conductivity | 29.1 W/m-K @Temperature 20.0 °C |
202 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Assab Steels 718HH Plastic Mold Material IMPAX SUPREME is a premium-quality vacuum-degassed Cr-Ni-Mo-alloyed steel which is supplied in the hardened and tempered condition. IMPAX SUPREME is manufactured to consistently high quality standar.. |
|||
Thermal Conductivity | 29.1 W/m-K @Temperature 704 °C |
202 BTU-in/hr-ft²-°F @Temperature 1300 °F |
|
Schmolz + Bickenbach Cryodur® 2363 (A-2) Cold Work Die Steel Description: Cryodur® 2363 is a cold-work steel developed for an excellent combination of wear resistance and toughness and Supplied in the annealed conditionCharacteristics: Good wear resistance; .. |
|||
Thermal Conductivity | 29.1 W/m-K @Temperature 21.1 °C |
202 BTU-in/hr-ft²-°F @Temperature 70.0 °F |
|
Schmolz + Bickenbach Holder Block Plastic Mold Steel Description: Holder Block is a modified AISI-4130 material with higher chromium and molybdenum content specifically designed holder steel for molds and dies and The material is forged on a 5000 ton.. |