Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.320 W/m-K @Temperature 450 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 842 °F |
|
Pyrotek Pyrotherm M-68 Structural Insulation Board Pyrotherm M-68 is a calcium-silicate board designed for non-ferrous applications. M-68 offers a unique combination of low shrinkage, low thermal conductivity and non-wetting properties which make i.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 260 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Pyrotek Pyrocast 80 Lightweight Castable Refractory Pyrocast 80 is a lightweight, low cement, fused silica castable designed for moderate flow molten aluminum contact applications. Pyrocast 80 offers low thermal conductivity, excellent resistance to.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 23.0 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Along flow; ISO 22007-4 |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 250 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM D1530 |
3M Dyneon™ 1620 PTFE Powder
(discontinued **) Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 250 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM E1530 |
3M Dyneon™ 1641 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 250 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM E1530 |
3M Dyneon™ 1645 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 100 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1530 |
3M Dyneon™ CC603 PTFE, 15% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
Thermal Conductivity | 0.320 - 0.420 W/m-K @Temperature 600 °C |
2.22 - 2.91 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GI 28 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.320 - 0.420 W/m-K @Temperature 100 °C |
2.22 - 2.91 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 110 Refractory Insulating Castable Description: Golite 110 is composed of a light weight refractory aggregate plus several additives to improve the mechanical and refractory properties.Remarks: These values apply to cast products. Al.. |
|||
Thermal Conductivity | 0.320 - 0.420 W/m-K @Temperature 1000 °C |
2.22 - 2.91 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast GOLITE 135 RL C Refractory Insulating Castable Description: Golite 135 RL C is a coarse low iron light weight castable and combines a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast .. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 900 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Zircar Refractory Composites RS-99-60 Refractory Sheet ZRCI Refractory Sheet Type RS-99-60 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 1600 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 2910 °F |
parallel to thickness |
Zircar Refractory Composites RS-3000 ALUMINA FELT ZRCI Alumina Felt Type RS-3000 is 97% high purity alumina fiber, ceramic felt with less than 1% shot. Type RS-3000 is a strong, flexible material with fibers held together with an organic binder. It.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 538 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C182 |
BNZ Materials BNZ-26 HS Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 816 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C182 |
BNZ Materials BNZ-26 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 1000 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 1830 °F |
ASTM C182 |
BNZ Materials BNZP-23B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 600 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTM C182 |
BNZ Materials BNZP-26 Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 816 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C182 |
BNZ Materials C-22 Z Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 800 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 1470 °F |
ASTM C182 |
BNZ Materials Color A Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 400 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTM C182 |
BNZ Materials Color CA Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 816 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C182 |
BNZ Materials PA 20 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.320 - 0.420 W/m-K @Temperature 100 °C |
2.22 - 2.91 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE MW Refractory Insulating Castable Description: Golite MW (medium weight) is composed of a light weight refractory aggregate plus several additives to improve the mechanical properties.Remarks: These values apply to cast products. Al.. |