Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 700 °C |
181 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 900 °C |
181 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 700 °C |
181 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 900 °C |
181 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 700 °C |
181 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 900 °C |
181 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 900 °C |
181 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded, aged at 538°C (1000°F) for 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 900 °C |
181 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 900 °C |
181 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 700 °C |
181 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 900 °C |
181 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 700 °C |
181 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 700 °C |
181 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged at 649°C (1200°F) for 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged at 649°C (1200°F) for 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 200 °C |
181 BTU-in/hr-ft²-°F @Temperature 392 °F |
Hardened and Tempered |
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 900 °C |
181 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 900 °C |
181 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 700 °C |
181 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |