Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 23.4 W/m-K @Temperature 204 °C |
162 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
International Mold Steel Premium H13 Hot Work Die and Mold Steel Description: International Mold Steel's Premium H-13 is a chromium-based, hot work die and plastic mold steel designed for increased production rates and longer tool life. It meets the restricti.. |
|||
Thermal Conductivity | 23.3 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 204 °C |
162 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
Latrobe LSSâ„¢ H13 PQ Hot Work Tool Steel TLS H13 PQ is Premium Quality H13 hot work steel that is designed to meet the highest quality standards in the die casting industry, and to excel in the most demanding hot work tooling applications... |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 204 °C |
162 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
Latrobe LSSâ„¢ H13 Tool Steel (ASTM H13) TLS H13 tool steel is a versatile chromium-molybdenum hot work steel that is widely used in hot work and cold work tooling applications. The hot hardness (hot strength) of H13 resists thermal fatigu.. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 204 °C |
162 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
Latrobe Viscount 20® Free Machining Tool Steel (ASTM H13S) Viscount 20 tool steel is a resulfurized H13 tool steel. The distribution of alloy sulfide particles in the microstructure enhances the machinability of the steel in the annealed condition. In addi.. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 900 °C |
162 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes 625SQ® Nickel Alloy Sheet Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649Â.. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 204 °C |
162 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
Latrobe Viscount 44® Prehardened Tool Steel (ASTM H13S) Viscount 44 is a free-machining, prehardened, H13-type hot work tool steel. It is produced using special melting, forging, and heat treating processes which provide the optimum in control
and reprod.. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 15% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 15% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 25% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 25% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 35% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 35% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 45% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 45% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 53% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 55% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 65% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 33%, Aged 565°C/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 23.4 W/m-K @Temperature 649 °C |
162 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 53%, Aged 565°C/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |